Page 1 of 3
H2a restoration
Posted: Sat May 02, 2009 3:16 pm
by nogger
Posted: Sat May 02, 2009 3:28 pm
by nogger
Posted: Sat May 02, 2009 4:40 pm
by TallyB
Looking good.

Posted: Sat May 02, 2009 9:23 pm
by Wolfie
Too late now Nogger we've all seen the Hammer.
Yep she's coming along nicely, but there less than fortnight now, you'll have to pull your finger out mate. 
Posted: Mon May 04, 2009 10:22 pm
by Nick13
That's some wicked ally polishinng matey.........
I take it there's a little more than Solvol involved there?

Posted: Tue May 05, 2009 10:01 pm
by Posh Pete
Lot of H2A's being restored lately. There were two nice ones at Donnington and I know of one other in the mix.
Very pleased with mine too.
Look forward to seeing this latest effort when it is finished.

Posted: Tue May 05, 2009 11:32 pm
by simonh
thats not a big hammer son

Posted: Fri Nov 20, 2009 5:14 pm
by nogger
Posted: Fri Nov 20, 2009 5:38 pm
by nogger
Oh before you ask YES I have a petrol cap just wanted to get it started ASAP, it started after a few kicks. got no gears tho so I could'nt tear it up the street hope it's just a linkage problem rather than full strip.
Posted: Fri Nov 20, 2009 7:30 pm
by Rubbadub
I do hope you will be refitting that natty backrest, very 1970s
Posted: Fri Nov 20, 2009 7:42 pm
by kas750
wonder if johnakay made it

Posted: Fri Nov 20, 2009 7:44 pm
by g6mow
Ouch !!!!

Posted: Fri Nov 20, 2009 9:24 pm
by BRN2DRL
Posted: Sat Nov 21, 2009 2:41 pm
by nogger
Posted: Sat Nov 21, 2009 9:13 pm
by Luke Sharp
nogger wrote:The cases after cleaning
Nogger, how did you do that with the cases?

Posted: Sat Nov 21, 2009 9:26 pm
by nogger
I boxed all the cases up and sent them to steve smethurst to get vapour blasted and a very good job he does also.
Posted: Sat Nov 21, 2009 9:41 pm
by robh1f
Luke it looks like aquablasting ...water and fine glass beads, had my h1 crankcases done a while ago came out suberbly!! any oil just wipes off with NO marks afterwards!
Posted: Sat Nov 21, 2009 9:46 pm
by robh1f
Wow Nogger went to get a fresh glass of red and finish my reply and you replied!!! well it was your post!! I'm guessing aqua and vapour are the same non??
Posted: Sun Nov 22, 2009 10:24 am
by malc87
nogger wrote:I boxed all the cases up and sent them to steve smethurst to get vapour blasted and a very good job he does also.
what did it cost?
Posted: Sun Nov 22, 2009 12:28 pm
by nogger
Hi Malc, Remember me from the Blackpool rally the 'bikeless' geordie lad well this is it finally running, notice I say running not going as I can't get gears at the mo but should sort it when I get chance. I wasn't ready for the rallies this year but next year HAHA

Can't wait.
Anyway to answer your question it was about £400 but that was all the cases and barrels blasted also all the polishing you see in the pics not cheap but I don't have time or facility to do anthing else .............. I KNOW I JUST PUT IT TOGETHER !!!!!
Is that cheating

Posted: Sun Nov 22, 2009 12:55 pm
by mal71
No , Just sensible mate.

Posted: Sun Nov 22, 2009 1:32 pm
by malc87
nogger wrote:Hi Malc, Remember me from the Blackpool rally the 'bikeless' geordie lad well this is it finally running, notice I say running not going as I can't get gears at the mo but should sort it when I get chance. I wasn't ready for the rallies this year but next year HAHA

Can't wait.
Anyway to answer your question it was about £400 but that was all the cases and barrels blasted also all the polishing you see in the pics not cheap but I don't have time or facility to do anthing else .............. I KNOW I JUST PUT IT TOGETHER !!!!!
Is that cheating

course i remember you from the blackpool rally
now you just need to write about the restoration for the club magazine